Overview of Inconel 939 Alloy Parts Developed by Additive Manufacturing Process

942
2024-12-10 12:00:28
查看翻譯

The related paper was published in Heliyon under the title "A systematic review of Inconel 939 alloy parts development via additive manufacturing process".

IN939 is a modern nickel based high-temperature alloy that can work continuously at high temperatures due to its excellent fatigue resistance, creep resistance, and corrosion resistance. The unique performance of IN939 is related to the composition of the alloy and specific post-treatment processes (such as solution treatment and aging treatment), resulting in features such as γ 'residues and MC and M23C6 carbides. This also includes the lack of eutectic and primary melting phases. For this alloy, the main component development is carried out through the powder bed melting process using a laser powder bed melting machine. Meanwhile, a separate study emphasized the synthesis of EB-PBF devices. The additive manufacturing process of these alloys is hindered by machine parameters, which have been found to be unable to obtain fully dense structures with the required properties alone. The purpose of these parameters is to improve its core performance while minimizing defects related to powder metallurgy processes, such as porosity, harmful precipitation, grain anisotropy, etc. This study aims to provide an overview of research progress related to IN939, with a clear focus on benchmarks achieved through additive manufacturing technology. Researchers discussed the work done in this field, compared the results of different studies, and identified gaps in current research. Through these works, researchers aim to gain a comprehensive understanding of the potential of IN939 and its applications in extreme environments.



Figure 1. Main aspects of developing IN939 components.

 


Figure 2. Microstructure of the casting sample.


Figure 3. Microstructure of the sample annealed at 1100 ℃ for 4 hours and then water quenched.


Figure 4. Main categories and software usage of additive manufacturing.


Figure 5. Simple schematic diagram of selective laser melting process for metal/alloy parts.


Figure 6. Schematic diagram of electron beam melting process.


Figure 7. Schematic diagram of direct energy deposition through (a) powder material feeding and (b) metal wire material feeding.


Figure 8. Schematic diagram of metal adhesive spraying process.


Figure 9. Fracture surfaces of (a) undisturbed specimen, (b) LTH specimen, (c) HTH specimen, and (d) cast LTH specimen subjected to creep rupture at 816 ℃/250 MPa.


Figure 10. Optical image of partially recast layer of the sample.


Figure 11. Scanning electron microscopy images of SLM samples (a, b) after aging without solution treatment, (c) after solution treatment+aging.


Figure 12. a, b) Cut the pit thickness and recast area of the sample. (c) Optical microscope images of the recast layer and HAZ area of CFG and (d) wire EDM methods.


Figure 13. Scanning electron microscopy microstructure images of the sample at different heights (b, c) 40mm, (d, e) 30mm, (f, g) 20mm, and (h, i) 10mm along the molding direction.


Inconel 939 additive manufacturing has been explored for advanced applications, which has led to further exploration of the impact of components and process parameters on this age hardening alloy. However, finished IN939 samples typically exhibit residual thermal strain, stress, and porosity, which may have a negative impact on their performance. To address these challenges, post-processing is considered crucial in achieving sample homogenization, controlling its microstructure, and reducing porosity. Although these processing methods have many benefits, they often require multiple steps and complex loops to form the required stages. These advances in AM and post-processing technology are expected to broaden the application range of IN939 parts and improve their performance in extreme environments. However, in addition to optimizing the microstructure and mechanical properties of IN939 parts, the performance of IN939 parts still needs to be further improved. Researchers can develop more targeted methods to optimize the performance of IN939 components and expand their potential applications by understanding their behavior in extreme environments rather than current developments. Combining hot isostatic pressing with optimized parameters at different stages of the multi-step heat treatment process can result in components with uniform microstructure and excellent isotropic mechanical properties.

Source: Yangtze River Delta Laser Alliance

相關推薦
  • Van's updates the manufacturer of laser-cut parts

    Van's Aircraft has responded to reports of ruptured dented parts found in AirVenture's latest kit. These defects are caused by external suppliers changing the process of laser cutting parts. From February 2022 to June 2023, Van's moved some parts from traditional punch manufacturing to an outside supplier that can laser cut rivet holes. The move is designed to increase the company's throughput and...

    2023-08-04
    查看翻譯
  • Microcomb launches a simplified design for powerful lasers based on chips

    Researchers at the University of Rochester have created new micro comb lasers that go beyond previous limitations and have simple designs suitable for various applications. The research results are published in Nature Communications.Optical frequency combs are optical measurement instruments that have revolutionized atomic clocks, spectroscopy, metrology, and other fields. However, the difficulty ...

    2024-05-25
    查看翻譯
  • Advanced optical giant Schott announces completion of Malaysia factory

    Recently, German optical giant SCHOTT is pleased to announce that its advanced production plant located in Gulim, Kedah, Malaysia has been successfully completed. This milestone event was celebrated with the joint witness of employees, clients, and representatives from the Malaysian Investment Development Authority (MIDA).The completion of the new factory marks a significant increase in Schott's...

    2024-10-16
    查看翻譯
  • Application of Laser Welding Technology in Ceramic Substrate Industry

     Ultra short laser pulses for local welding (Source: Fraunhofer IOF)With the accelerated evolution of electronic devices towards high power, high frequency, and miniaturization, ceramic substrates have become core materials in fields such as power semiconductors, 5G communications, and new energy vehicles due to their excellent thermal conductivity, insulation, and high temperature resistance. H...

    03-17
    查看翻譯
  • Chip based comb laser illumination and unlocking of new applications

    Researchers have shown that dissipative Kerr solitons (DKS) can be used to create chip based optical frequency combs with sufficient output power for optical atomic clocks and other practical applications. This progress may lead to chip based instruments being able to perform precise measurements that were previously only possible in a few specialized laboratories.Gr é gory Moille from the ...

    2023-08-30
    查看翻譯