I have a breakpoint when using RDWelder-SW laser welding

Every

My control system is RDWelder-SW, but the welding efficiency is not good, with breakpoints and significant laser splashing. What should I do to troubleshoot or optimize? Thank you!

你能回答这个问题吗?

请写下你的答案,帮助遇到同样问题的用户。

回答(2)

  • Williams
    已采纳回答已采纳回答

    Adjust the focus to the appropriate position, increase the laser power, and adjust the swing length and frequency

    1
    回复
    • I tried increasing the laser power while adjusting the swing amplitude and frequency, and now the welding results are much better.

      0
      回复
  • Is the use of protective gas correct? For stainless steel or carbon steel, the recommended argon flow rate is 15-25 L/min, and the purity of argon must be high (≥ 99.99%)

    1
    回复
    • Yes, the handling of the shielding gas is correct.

      0
      回复